The desired casting mud is prepared by mixing water and color pigment into the mud taken powdery from France.
After the mud rested for 1 week and reaches the appropriate consistency, it is poured into plaster molds and the shaping process is completed.
The mud, which takes the form of the mold, is expected to dry sufficiently. Then it is removed from the mold and retouching are performed.
The first firing process is done at 980 degrees. The biscuit products are sanded and prepared for glazing. The biscuit products are sanded and prepared for glazing.
Handmade products with transparent, matte or glossy glaze are fired between 1220 and 1250 degrees.
Fired products are branded and fired again at 600 degrees to complete the marking process. Then It is sanded again to make unglazed surfaces smooth and the final product is obtained.